this post was submitted on 18 Oct 2024
17 points (94.7% liked)

3DPrinting

15618 readers
354 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: [email protected] or [email protected]

There are CAD communities available at: [email protected] or [email protected]

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS
17
submitted 1 month ago* (last edited 1 month ago) by csm10495 to c/[email protected]
 

Hey folks,

I'm not sure what I'm doing wrong. I'm printing PETG (https://kingroon.com/collections/petg-filament?) on my Neptune 3 Plus. It's sort of like it starts (almost) ok, sticks to the plate just fine, then a few layers up it seems to almost have inconsistent extrusion (or maybe even trouble pulling the filament?) leading to holes, etc. till the model just falls apart. See linked photos for about where I give up each time.

I'm printing with Cura and 240C printing, 90C on the build plate. 45mm/s (I've gone down from 60mm/s). Retraction on, no z-hop. 60% fan, though I've tried it with 20% and 100% fan as well.

The filament is in a dryer at 55C. Funny enough I printed basically perfectly (without drying, straight out of the bag) with default settings the first time I printed. The second time and on, have had this problem... and have had it in the dryer.

Any ideas would be much appreciated. Thanks!

Edit: In case its useful, I'm printing this piece: https://file.io/D9jxYq4KOrL7 which is a small remix of a piece from https://www.printables.com/model/130507-bolt-action-pen-for-pilot-g2-cartridges

you are viewing a single comment's thread
view the rest of the comments
[–] [email protected] 1 points 1 month ago

This looks like heat creep and/or clog. Check the hotend fan (not the part cooling one). If it starts happening after a while, it's either that or the nozzle has cooled too much. But if it happens with lower speed as well, then I wouldn't say it's that it's the latter. Try increasing the temperature. I'm printing mine at 270°C. Also I keep the bed at 70°C but that's not important. I've had issues like that with bad conducting nozzles (hardened/stainless steel) and thermistors not properly seated on the heat block. When this happens, pause the print, try feeding the filament by hand and see if there is any resistance (can you feel the clog). Try increasing the temperature, reduce the retraction distance to try and avoid it. I'm printing exclusively with petg for years now, never had issues like this due to moisture. You get more stringing, yes, but no failures on actual printing.