this post was submitted on 11 Jul 2023
13 points (100.0% liked)

3DPrinting

15661 readers
30 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: [email protected] or [email protected]

There are CAD communities available at: [email protected] or [email protected]

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 2 years ago
MODERATORS
13
Tips for PETG? (lemmy.world)
submitted 1 year ago* (last edited 1 year ago) by [email protected] to c/[email protected]
 

Im very new to 3d printing and this is my first time using anything other than pla. So far all of my prints are lifting off the bed at the corners. They start off looking beautiful. No stringing, great adhesion, etc. But after a few layers, they start to come off. Especially on larger prints.

Heres my setup:

  • Ender 3 pro with skr mini e3 v2
  • Creality Ender 3 glass bed upgrade
  • Bed temp: 90C
  • Extruder temp: 240C
  • Nozzle diameter: .4
  • Layer height: .2
  • First layer: .45
  • Speed: 60mm/s
  • Slicer: Silc3r

I realize that asking this question is like asking WebMD to dianose my sniffles, cause it can literally be anything, but Im hoping someone with more experience can give me some pointers on what works for them. Thanks yall!

Update: First of all, thank you all so much for the kick ass suggestions! I really appreciate all of your replies. Since pretty much everyone recommended it, I went ahead and got a textured spring steel PEI plate and holy shit, it didn't disappoint. Adhesion has been fantastic. I also ended up lowering my bed temp down to 75 from 90 and pushing my hotend temp to 245 for the first layer, then back to 240. I got an enclosure to help keep the plate clean but I also stocked up on some blue dawn dish soap. I still have a little more trial and error with print speed and cooling but I'm literally getting the best prints I've ever gotten thanks to all of your suggestions. Yall are awesome and I'm really glad I posted here.

you are viewing a single comment's thread
view the rest of the comments
[–] [email protected] 2 points 1 year ago (1 children)

That’s so strange, I have no problems printing PETG all the time.

Yeah, I don't know - I've never had any big issues in the past with it either (I mostly print PLA+ though, unless I need something more heat-resistant for my car or outdoor use).

This particular issue was with an Ender 3 V2 running a BLTouch and an aftermarket textured PEI sheet in an enclosure - so there were no drafts or anything that would explain the bad adhesion either. Just scrubbed it with some water and dish soap. That was literally the only thing I messed with between the spaghetti result run and a great first layer run, so I figured I'd mention it in case it might help OP.

[–] [email protected] 3 points 1 year ago

Ahhh, see from my Zortrax printer I learned that PETG benefits from no enclosure - drafts are fine. It actually helps increase print quality. I run my Prusa Mk3s printers with no enclosure (since I only use them for mainly PETG and TPU, and occasionally PLA). I have Zortrax printers for my ABS, ABS/PolyCarbonate Blends, and HIPS plastics (but holy hell I hate the closed software on the Zortrax printers and their Zsuite slicing software - absolute garbage which cripples printers that cost thousands of dollars - I can't even tweak temperature, fan speeds, flow rates, etc mid-print like literally every other printer I've handled over the past decade!).