this post was submitted on 05 Dec 2023
11 points (100.0% liked)

3DPrinting

15629 readers
202 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: [email protected] or [email protected]

There are CAD communities available at: [email protected] or [email protected]

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS
 

I apologize for the links below being vendor specific, but the linked products are the specific products I have used. I have no affiliation with the shop other than they offer to bill my job instead of having me pay upfront and then get the expenses redeemed. (I have tried making this both subscript and super script with respectively ^ and ~, but none works on lemmy)

I seek advice on proceeding with the setup and acquiring an acceptable printing quality.

Background

I have recently "upgraded" a creality cr6 se at work. I installed a spider steel/PEI plate (https://3deksperten.dk/products/spiderflexiplate-double-system-255x245-ex-cr-6-se), a bimetal heatbreak https://3deksperten.dk/products/3dsupreme-titanium-alloy-bi-metal-heatbreak-cr6-se) and a hardened steel nozzle (0.4mm from this kit https://3deksperten.dk/products/creality-3d-3d-printing-up-market-nozzle-kit-8-pcs)

Findings

Testing this new setup I used the PLA spool I had been printing with days before without issue. The new and old nozzles are all 0.4mm.

What I discovered was that I couldn't get any adhesion to the built plate, some spray glue (this exact make and model https://3deksperten.dk/products/printafix-100ml) fixed that. Then layer adhesion was an issue. So I upped the temp to the max for this PLA and increased the extrusion rate. First 10 layers or so were somewhat ok, but the rest delaminated instantly.

I then opened a brand new spool of PLA, thinking that the old spool had moisture issues. Cranked the temp to max, 210°C, added 5°C to the bed and applied a strong shot of spray glue. This time the print actually got done, but the parts where Cura's tree support was supposed to be supporting, the layers seem to come apart. The rest of the print was somewhat ok, though not great.

Current considerations

  • Maybe I attempted too much at the same time. I may try swapping the nozzle back and only deal with the plate and heatbreak.
  • The heat break may be install wrong. The nozzle was screwed in all the way, loosened a few turns, then the heat break was screwed in all the way. The nozzled was then tightened. No heating was done. I may try giving the heat break a few turns before installing the old nozzle again.
  • Should I have heated hotend before tightening the nozzle?
you are viewing a single comment's thread
view the rest of the comments
[–] [email protected] 1 points 11 months ago

Always heat up nozzle before tightening/untightening. And yeah up your temp or even better stick with brass nozzle for pla